| Mea | Kōho | 'Ikeʻike | |
| Huakai | Kg / m3 | ≤ 220 ± 10% | |
| Nui | Palena | mm | 600*300/900*300/1000*500 mānoanoa: 25-115 |
| Piku | Kani: 20- 2200mm mānoanoa: 25-100mm |
||
| Hanaʻia ka nui kūikawā e like me ke koi o ka mea kūʻai aku. | |||
| Ikaika ikaika | Mpa | ≥0.7 | |
| ʻO ka ikaika ikaika (min.) | Mpa | ≥0.35 | |
| Linear Shrinkge (max) | % | Ç2.0 | |
| Ka hana o ka Thermal Condertivity (Max.) | W / m.k | ≤ «.065 | |
| 'Templelo SERVAM. (Max) | ° C | 650-1000 | |
| Wahi a ka huahana e like me astm c 533 maʻamau. | |||
| Kaumakai | Kōho | Kuhikuhi | |||
| SIO2 | % | 44 | |||
| Caoo | % | 43 | |||
| Mgo | % | 1.3 | |||
| Kahuna Kahu | Kg / m³ | 220 ± 10% | |||
| ʻO keʻano hana | W / m.k | ≤ «.052 | |||
| Ikaika ikaika | Mpa | ≥0.50 | |||
| Ikaika ikaika | Mpa | ≥0.30 | |||
| Linear shrinkage | % | ≤ | |||
| Palena kala | 650 ° C | ||||
| Ka pohōʻana | 11.1% | ||||
| Long (± 3) mm | Mānoanoa (± 3) mm | ID (+2 -1.5mm) | |||
| 600 | ≥30 | 20--2200 | |||
| Hiki iā mākou ke hāʻawi i nā nui'ē aʻe e like me nā koina o nā mea kūʻai aku | |||||