| Project | Index / Indicator | |
| Bulk Density (kg/m³) | 600±10% | 900±10% |
| Compressive Strength for Thickness < 20 mm (15% Compression in Thickness Direction) (MPa) | ≥0.8 | ≥3.0 |
| Compressive Strength for Thickness ≥ 20 mm (15% Compression in Thickness Direction) (MPa) | ≥0.8 | ≥3.0 |
| Permanent Linear Change on Heating, % (1000℃ × 12h) | 0~-2 | 0~-2 |
| Thermal Conductivity, W/(m·K) (Hot Surface Temperature: 350℃) |
≤0.1 | ≤0.12 |
| Flexural Strength (MPa) | ≥2.0 | ≥3.0 |